Mechanical Properties | Metric | English | Comments |
---|---|---|---|
300% Modulus | 0.0113 GPa | 1.64 ksi | Injection molded parts; DIN 53504 |
Huntsman IROGRAN® A 85 P 5350 TPU-Polyester Introduction: IROGRAN A 85 P 5350 is a flame-retardant, halogen-free, polyether based thermoplastic polyurethane intended for extrusion and injection molding applications. IROGRAN A 85 P 5350 is par.. |
|||
300% Modulus | 0.0113 GPa | 1.64 ksi | Cured |
KKPC Kumho KHS 65 High Styrene Resin Masterbatch (HSR) High Styrene Resin Masterbatch (HSR)Characteristics: KOSYN KHS is produced by mixing SBR 1502 of 23.5% styrene and high styrene resin latex at high temperature. It works as plasticizer which improve.. |
|||
300% Modulus | 0.0113 GPa | 1.64 ksi | Cured |
KKPC Kumho KHS 65P High Styrene Resin Masterbatch (HSR) High Styrene Resin Masterbatch (HSR)Characteristics: KOSYN KHS is produced by mixing SBR 1502 of 23.5% styrene and high styrene resin latex at high temperature. It works as plasticizer which improve.. |
|||
300% Modulus | 0.0113 GPa | 1.64 ksi | Cured |
KKPC Kumho RM 21L High Styrene Resin Masterbatch (HSR) High Styrene Resin Masterbatch (HSR)Characteristics: KOSYN KHS is produced by mixing SBR 1502 of 23.5% styrene and high styrene resin latex at high temperature. It works as plasticizer which improve.. |
|||
300% Modulus | 0.0113 GPa | 1.64 ksi | |
Taiwan Sheen Soon Sheenthane® A8230 Thermoplastic Polyurethane Elastomer Thermoplastic polyurethane elastomer for injection moldingInformation provided by Taiwan Sheen Soon Co., LTD. |
|||
300% Modulus | 0.0113 GPa | 1.64 ksi | ASTM D412 |
Styron Sprintan® SLR 6430 Solution Styrene Butadiene Rubber (S-SBR) Composition: SPRINTAN® SLR-6430 – Schkopau is manufactured by anionic solution polymerization using an organo-lithium initiator. In relation to solid rubber the grade is extended with 37.5 p.. |