Mechanical Properties | Metric | English | Comments |
---|---|---|---|
300% Modulus | 0.0138 GPa | 2.00 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber, Hardness 66A MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
300% Modulus | 0.0138 GPa | 2.00 ksi | ASTM D412 |
SK Chemicals SKYTHANE® R190A Polyether Based Thermoplastic Polyurethane Elastomer Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets .. |
|||
300% Modulus | 0.0138 GPa | 2.00 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber, Hardness 66A MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
300% Modulus | 0.0138 GPa | 2.00 ksi | ASTM D412 |
Lubrizol ESTANE® 58237 Ether Based Thermoplastic Polyurethane Features: High moisture vapor transmission. Good physical properties and elasticity.Uses: Blown and flat die/cast film extrusion.Available in Americas, Europe, Middle East, Africa, India and AsiaInf.. |
|||
300% Modulus | 0.0138 GPa | 2.00 ksi | ASTM D412 |
Lubrizol Estane® AG 8451 Thermoplastic Polyurethane Type: Estane® AG 8451 is a polyether based aliphatic (TPU) specifically formulated to be used as an adhesive interlayer film. AG-8451 is an excellent general purpose polymer for all optical allpha.. |
|||
300% Modulus | 0.0138 GPa | 2.00 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with Benzoflex T-150 Plasticizer MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
300% Modulus | 0.0138 GPa | 2.00 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber, 0.35 PHR Caytur 4 MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
300% Modulus | 0.0138 GPa | 2.00 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with Benzoflex T-150 Plasticizer MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
300% Modulus | 0.0138 GPa | 2.00 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber, 0.35 PHR Caytur 4 MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |