300% Modulus 0.0141 GPa
2.04 ksi
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer with 6 PHR Varox DBPH-50
MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c..
300% Modulus 0.0141 GPa
2.04 ksi
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer with 6 PHR Varox DBPH-50
MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c..