Polymer Property : 300% Modulus = 2.11 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
300% Modulus 0.0145 GPa
2.11 ksi
KKPC KOSYN SOL 5520 Solution Styrene Butadiene Rubber (S-SBR)
Solution Styrene Butadiene Rubber (S-SBR)Characteristics: This product is made by solution polymerization under which styrene and butadiene react in organic solvent using alkyl-lithium catalyst. It ..