Mechanical Properties | Metric | English | Comments |
---|---|---|---|
300% Modulus | 0.0146 GPa | 2.12 ksi | |
KKPC KOSYN SOL 5001 Solution Styrene Butadiene Rubber (S-SBR) Solution Styrene Butadiene Rubber (S-SBR)Characteristics: This product is made by solution polymerization under which styrene and butadiene react in organic solvent using alkyl-lithium catalyst. It .. |
|||
300% Modulus | 0.0146 GPa | 2.12 ksi | |
KKPC KOSYN SOL 5740 Solution Styrene Butadiene Rubber (S-SBR) Solution Styrene Butadiene Rubber (S-SBR)Characteristics: This product is made by solution polymerization under which styrene and butadiene react in organic solvent using alkyl-lithium catalyst. It .. |