Mechanical Properties Metric English Comments
300% Modulus 0.0156 GPa
2.26 ksi
aged 70 hours at 250ºF in ASTM Oil #901
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer with 20 PHR HAF Black (Typical)
MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c..
300% Modulus 0.0156 GPa
2.26 ksi
ASTM D412
Styron Sprintan® SLR 4601 Solution Styrene Butadiene Rubber (S-SBR)
Composition: SPRINTAN® SLR-4601 – Schkopau is manufactured by anionic solution polymerization using an organo-lithium initiator. The product has a medium styrene/high vinyl micro structure a..
300% Modulus 0.0156 GPa
2.26 ksi
aged 70 hours at 250ºF in ASTM Oil #901
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer with 20 PHR HAF Black (Typical)
MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c..
300% Modulus 0.0156 GPa

@Temperature 145 °C,
Time 2990 sec
2.26 ksi

@Temperature 293 °F,
Time 0.830 hour
cured; ASTM D412
LG Chemical NBR 6850 High Acrylonitrile Polymer
Description: NBR 6850 is a copolymer of butadiene and acrylonitrile manufactured by advanced emulsion polymerization technology of Goodyear and LG Chem. NBR 6850 is a non staining, medium mooney, an..