Mechanical Properties Metric English Comments
300% Modulus 0.01663 GPa
2.412 ksi
ASTM D412
Lubrizol Advanced Materials Pearlthane® 12T92E Thermoplastic Polyurethane Elastomer
PEARLTHANE® 12T92E is a special polyester-based TPU, supplied in form of translucent, colorless pellets, combining hardness with excellent processability and low temperature performance. This gra..