Mechanical Properties Metric English Comments
300% Modulus 0.0183 GPa
2.65 ksi
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 50 PHR N774 (SRF) Filler
MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st..
300% Modulus 0.0183 GPa
2.65 ksi
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 50 PHR N774 (SRF) Filler
MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st..
300% Modulus 0.0183 GPa
2.65 ksi
aged in air at 100ºC for 4 days
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with TCP Plasticizer
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..
300% Modulus 0.0183 GPa
2.65 ksi
aged in air at 100ºC for 4 days
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with TCP Plasticizer
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..