Mechanical Properties | Metric | English | Comments |
---|---|---|---|
300% Modulus | 0.0197 GPa | 2.85 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 90 PHR N650 Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
300% Modulus | 0.0197 GPa | 2.85 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 45 PHR N220 Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
300% Modulus | 0.0197 GPa | 2.85 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 90 PHR N650 Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
300% Modulus | 0.0197 GPa | 2.85 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 45 PHR N220 Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |