Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : 300% Modulus = 3.48 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
300% Modulus 0.0240 GPa
3.48 ksi
ISO 37
Huntsman AVALON® 98 AE Thermoplastic Polyurethane
Introduction: AVALON 98 AE is a general purpose polyester based thermoplastic polyurethane for injection molding. AVALON 98 AE is part of the AVALON Perform Range and offers a premium soiling materi..
300% Modulus 0.0240 GPa
3.48 ksi
ASTM D412
Lubrizol Advanced Materials PEARLTHANE® D16N98UV Thermoplastic Polyurethane Elastomer
Pearlthane® D16N98UV is a polyether-based TPU, supplied in form of transparent, colorless pellets, combining high hardness with excellent mechanical properties and good hydrolysis and microbial r..
300% Modulus 0.0240 GPa
3.48 ksi
ISO 37
Huntsman AVALON® 95 AB Thermoplastic Polyurethane
Introduction: AVALON 95 AB is a high performance polyester based thermoplastic polyurethane for injection molding. AVALON 95 AB is part of the AVALON Performance Range and offers a premium soling ma..
300% Modulus 0.0240 GPa
3.48 ksi
DIN 53504
Huntsman IROGRAN® A 92 E 4738 Polyester-Based TPU-Injection Extrusion Grade
Introduction: IROGRAN A 92 E 4738 is a white-colored, thermoplastic special-polyester-polyurethane for injection molding applications. Additional characteristics of the product are flexibility and h..
300% Modulus 0.0240 GPa
3.48 ksi
ASTM D412
Lubrizol ESTANE® 58130 Ester Based Thermoplastic Polyurethane
Features: Fast cycling, broad temperature performance, and durabilityUse: Injection Molding.Available in Americas, Europe, Middle East, Africa, India and AsiaInformation provided by Lubrizol
300% Modulus 0.0240 GPa
3.48 ksi
ISO 37
Huntsman AVALON® 95 ABR Thermoplastic Polyurethane
Introduction: AVALON 95 AB is a high performance polyester based thermoplastic polyurethane for injection molding. AVALON 95 AB is part of the AVALON Performance Range and offers a premium soling ma..
Copyright © lookpolymers.com All Rights Reserved