Mechanical Properties Metric English Comments
300% Modulus 0.02801 GPa
4.063 ksi
ISO 527-2/5A/500
Lubrizol Advanced Materials PEARLTHANE® 11T60D Thermoplastic Polyurethane Elastomer
Type : Pearlthane® 11T60D is a polycaprolactone copolyester-based thermoplastic polyurethane.Main Application : Injection MouldingSpecial Features : Combining very high hardness with excellent me..