Polymer Property : 300% Modulus = 5.37 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
300% Modulus 0.0370 GPa
5.37 ksi
ISO 527-2/5A/500
Lubrizol Advanced Materials Pearlthane® ECO D12T55D Thermoplastic Polyurethane
Type: Pearlthane® ECO D12T55D is a high performance bio-based thermoplastic polyurethane. With ca. 29% bio-based content.Main Application : Extrusion/MouldingSpecial Features : Properties similar..
300% Modulus 0.0370 GPa
5.37 ksi
ASTM D412
Wanhua Chemical Wanthane® WHT-1172 Polyester Based TPU
Excellent mechanical properties, high abrasion resistance, tear resistance, short cycle timeInformation provided by Wanhua Chemical Group Co., Ltd.