300% Modulus 0.0400 GPa
5.80 ksi
ASTM D412
SK Chemicals SKYTHANE® S155D Polyester Based Thermoplastic Polyurethane Elastomer
Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets ..
300% Modulus 0.0400 GPa
5.80 ksi
ASTM D412
Wanhua Chemical Wanthane® WHT-1564 Polyester Based TPU
Low cost, good mechanical properties, good processabilityInformation provided by Wanhua Chemical Group Co., Ltd.