Polymer Property : Impact Test = 0.295 ft-lb Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Impact Test 0.400 J

@Thickness 3.17 mm,
Temperature 22.8 °C
0.295 ft-lb

@Thickness 0.125 in,
Temperature 73.0 °F
150 in/sec; ASTM D-3763
Chevron Phillips K-Resin® KR01BR SBC  (discontinued **)
K-Resin® Styrene-Butadiene Copolymer (SBC)Applications:Molded boxes with integral hingesMedical devicesDisplaysToysMedia packagingFeatures:Good stiffnessGood toughnessGood warpage resistanceExcelle..