Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Impact Test | 0.600 J | 0.443 ft-lb | Instrumented Dart Impact (Energy at Peak Force); ASTM Test |
Styrolution Styrolux 656C SBC Styrolux 656C is a high flow thermoplastic injection molding styrene-butadiene block copolymer. It has crystal clarity, good toughness, good stiffness, and warpage resistance for general molding ap.. |
|||
Impact Test | 0.600 J | 0.443 ft-lb | unspecified impact test |
Du-Co Ceramics CS-144-L-5 Steatite Properties reported below are averages from unglazed specimens. Tests performed to ASTM specifications. Actual values may vary. Information provided by DU-CO Ceramics Company. |