Polymer Property : Impact Test = 0.560 J Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Impact Test 0.560 J
0.413 ft-lb
unspecified impact test
Du-Co Ceramics DC-16-L-3 Steatite
Properties reported below are averages from unglazed specimens. Tests performed to ASTM specifications. Actual values may vary. Information provided by DU-CO Ceramics Company.
Impact Test 0.560 J
0.413 ft-lb
unspecified impact test
Du-Co Ceramics DC-9-L-3 Steatite
Properties reported below are averages from unglazed specimens. Tests performed to ASTM specifications. Actual values may vary. Information provided by DU-CO Ceramics Company.