Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Impact Test | 1.60 J | 1.18 ft-lb | Spencer Impact ASTM D3420 |
DuPont™ Clysar® HP Polyolefin Shrink Packaging Film, 100 Gauge
(discontinued **) Data provided by DuPont Packaging Polymers.A strong, clear, biaxially oriented, heat-shrinkable, linear low-density polyolefin film. Cross-linking produces a film that is extremely rugged and durab.. |
|||
Impact Test | 1.60 J | 1.18 ft-lb | Spencer Impact ASTM D3420 |
DuPont™ Clysar® LLP Polyolefin Shrink Packaging Film, 100 Gauge
(discontinued **) Data provided by DuPont Packaging Polymers.A strong, clear, biaxially oriented, nonirradiated, heat-shrinkable, linear low-density polyolefin film. LLPS is the silicon treated, hot slip version of .. |
|||
Impact Test | 1.60 J | 1.18 ft-lb | Dynatest, Penetration Energy; ISO 7765-2 |
Borealis Borsoft™ SD200CF High Impact Polypropylene Random Heterophasic Copolymer for Cast Film Borsoft SD200CF is a very soft random heterophasic copolymer, suitable for use on chill roll process. The product combines unique softness with outstanding mechanical properties making it the ideal.. |