Polymer Property : Impact Test = 11.3 J Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Impact Test 5.65 - 11.3 J
4.17 - 8.33 ft-lb
Torque Break
Ritelok TL22 Screwlock
Anaerobic. Low strength threadlocker for fasteners less than 1/4". Prevent corrosion, Vibration resistant, Dismantle using normal tools
Impact Test 2.26 - 11.3 J
1.67 - 8.33 ft-lb
Torque Break
Ritelok TL90 Post Assembly Threadlocker
Anaerobic. Low viscosity threadlocker for port assembly. High torque strength, Prevent corrosion, Locks solid-will not dismantle, Vibration resistant
Impact Test 2.26 - 11.3 J
1.67 - 8.33 ft-lb
Break
ND Industries 150 Wicking Adhesive Sealant Threadlocker
General DescriptionMedium to high strength. Locks pre-assembled fasteners through capillary action and seals porosities in welds and hairline cracks in castings.Meets military spec MIL-S-46163 Type..
Impact Test 5.65 - 11.3 J
4.17 - 8.33 ft-lb
Break
ND Industries ScrewGrade® 111 Removable Threadlocker
A low strength threadlocker which eliminates vibrational loosening, and seals against leakage and corrosion.Typical Usessoft metal fasteners, precision screws, and locking fasteners smaller than .25..