Polymer Property : Impact Test = 134 J Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Impact Test 134 J
98.8 ft-lb
Multiaxial Impact; ISO 6603
SABIC Innovative Plastics Lexan® HFD1014 PC Copolymer (Asia Pacific)
7 MFR LEXAN HFD Copolymer
Impact Test 134 J
98.8 ft-lb
Multiaxial Impact; ISO 6603
SABIC Innovative Plastics Lexan® HFD1014 PC Copolymer (Europe-Africa-Middle East)
7 MFR LEXAN HFD Copolymer
Impact Test 134 J
98.8 ft-lb
Multiaxial Impact; ISO 6603
SABIC Innovative Plastics Lexan® HFD1034 PC Copolymer
7 MFR LEXAN HFD Copolymer UV-stabilized, available in transparent colors only
Impact Test 134 J
98.8 ft-lb
Multiaxial Impact; ISO 6603
SABIC Innovative Plastics Lexan® HFD1034 PC Copolymer (Asia Pacific)
7 MFR LEXAN HFD Copolymer UV-stabilized, available in transparent colors only
Impact Test 134 J
98.8 ft-lb
Multiaxial Impact; ISO 6603
SABIC Innovative Plastics Lexan® HFD1034 PC Copolymer (Europe-Africa-Middle East)
7 MFR LEXAN HFD Copolymer UV-stabilized, available in transparent colors only
Impact Test 134 J
98.8 ft-lb
Multiaxial Impact; ISO 6603
SABIC Innovative Plastics Lexan® EXRL0684 PC Copolymer
7 MFR LEXAN High Flow Ductile CopolymerThis data was supplied by SABIC-IP for the Americas region.
Impact Test 134 J
98.8 ft-lb
Multiaxial Impact; ISO 6603
SABIC Innovative Plastics Lexan® HFD1014 PC Copolymer
7 MFR LEXAN HFD Copolymer