Mechanical Properties Metric English Comments
Impact Test 244 J

@Thickness 6.35 mm
180 ft-lb

@Thickness 0.250 in
ARM
ExxonMobil HDPE HD 8660.29 High Density Polyethylene Resin
Product Description: HD 8660 series are high density hexane copolymers designed to offer superior toughness and stiffness. They are ideally suited for applications that require the optimum balance o..
Impact Test 244 J

@Thickness 6.35 mm
180 ft-lb

@Thickness 0.250 in
ARM
ExxonMobil HDPE HD P8660.29 High Density Polyethylene Resin
Product Description: HD 8660 series are high density hexane copolymers designed to offer superior toughness and stiffness. They are ideally suited for applications that require the optimum balance o..
Impact Test 244 J

@Thickness 6.35 mm,
Temperature -40.0 °C
180 ft-lb

@Thickness 0.250 in,
Temperature -40.0 °F
Impact Strength; Max Force; ARM
ExxonMobil Escorene® LL-8302 LMDPE Rotational Molding Grade  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.LL-8300 series are linear medium density polyethylene resins that provide outstanding environmental stress crack resistance. LL-8302 is the base re..
Impact Test 244 J

@Thickness 6.35 mm,
Temperature -40.0 °C
180 ft-lb

@Thickness 0.250 in,
Temperature -40.0 °F
Impact Strength; Max Force; ARM
ExxonMobil Escorene® LL-8361 LMDPE Rotational Molding Grade  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.LL-8300 series are linear medium density polyethylene resins that provide outstanding environmental stress crack resistance. LL-8361 is fully formu..