Mechanical Properties Metric English Comments
Impact Test 27.0 J

@Temperature 0.000 °C
19.9 ft-lb

@Temperature 32.0 °F
multiaxial, 15 mph; ASTM D3763
Solvay Engineered Polymers SEQUEL® 2325 Engineered Polyolefin  (discontinued **)
Description: SEQUEL® 2325 engineered polyolefin is designed for mold-in-color automotive interior applications. This material exhibits excellent low-gloss surface appearance and processability. Ap..
Impact Test 27.0 J

@Temperature 0.000 °C
19.9 ft-lb

@Temperature 32.0 °F
multiaxial, 15 mph; ASTM D3763
Solvay Engineered Polymers SEQUEL® 2382 Engineered Polyolefin  (discontinued **)
Description: SEQUEL® 2382 engineered polyolefin is designed for large mold-in-color interior applications that require stiffness and dimensional stability. This material exhibits excellent process..
Impact Test 27.0 J

@Temperature -29.0 °C
19.9 ft-lb

@Temperature -20.2 °F
Montell drop weight impact strength
LyondellBasell Pro-fax SB787 Polypropylene Impact Copolymer
Key Features: blush resistance, excellent dimensional satiability, fast cycling, easy molding, good cold impact resistance, good stiffness and impact balance, easily colored, FDA acceptableApplicati..
Impact Test 27.0 J

@Temperature 23.0 °C
19.9 ft-lb

@Temperature 73.4 °F
Instrumented Impact Energy @ peak; ASTM D 3763
SABIC Innovative Plastics LNP Lubricomp YP003 TPEE
LNP LUBRICOMP* YP003 is a compound based on TPEE resin containing PTFE, Silicone. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP for the Americas ..
Impact Test 27.0 J
19.9 ft-lb
Multiaxial Impact; ISO 6603
SABIC Innovative Plastics LNP STAT-KON DX00887C PC
LNP STAT-KON* DX00887C is a compound based on Polycarbonate resin containing Proprietary Filler(s). Added features of this material include: Clean Compounding System, Electrically Conductive.
Impact Test 27.0 J
19.9 ft-lb
Multiaxial Impact; ISO 6603
SABIC Innovative Plastics LNP STAT-LOY 9X07438 ASA+PC
LNP* STAT-LOY* 9X07438 is a compound based on Polycarbonate/ASA containing Proprietary Filler(s). Added features of this grade include: Antistatic, Colorable, Weatherable.
Impact Test 27.0 J
19.9 ft-lb
ASTM D3763
ExxonMobil Exxtral™ H1025 Performance Polyolefin
Product Description: A specialty thermoplastic olefin resin with good flow, cold temperature impact resistance, low CLTE, and excellent paintability for automotive exterior applications.Availability..
Impact Test >= 27.0 J

@Temperature -40.0 °C
>= 19.9 ft-lb

@Temperature -40.0 °F
from AM 611; EN 10045-1
Outokumpu LDX 2101® Duplex Stainless Steel
Applications: Pulp and paper industryDesalination plantsFlue-gas cleaningCargo tanks and pipe systems in chemical tankersSeawater systemsFirewalls and blast walls on offshore platformsBridgesCompone..