Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Impact Test | 2.36 J | 1.74 ft-lb | Multi-Axial Instrumented Impact Energy; ISO 6603-2 |
LNP Lubricomp® PDX-J-91198 Polyethersulfone, Proprietary Filler
(discontinued **) Features: LubricatedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still ac.. |