Mechanical Properties Metric English Comments
Impact Test 3.52 J
2.60 ft-lb
Multi-Axial Instrumented Impact Energy; ISO 6603-2
LNP Thermotuf® QF-1006 HI Polyamide 6/10 Copolymer, Glass Fiber Reinforcement  (discontinued **)
Features: High Impact ResistanceForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades ..