Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Impact Test | 217 J @Thickness 6.35 mm |
160 ft-lb @Thickness 0.250 in |
Compression Molded; ARM Method |
NOVA Chemicals Surpass® RMs244-UG Octene sHDPE Rotational Molding Film Features: Octene copolymerExceptional low temperature propertiesOutstanding stiffnessBroad processing windowSuperior whiteness for improved part appearanceEasy mold releaseNSF listed for Standards 1.. |
|||
Impact Test | 217 J @Thickness 6.35 mm |
160 ft-lb @Thickness 0.250 in |
Compression Molded; ARM Method |
NOVA Chemicals Surpass® RMs244-U Octene sHDPE Rotational Molding Film Features: Octene copolymerExceptional low temperature propertiesOutstanding stiffnessBroad processing windowSuperior whiteness for improved part appearanceEasy mold releaseNSF listed for Standards 1.. |
|||
Impact Test | 217 J @Thickness 25.4 mm |
160 ft-lb @Thickness 1.00 in |
Falling Dart; ASTM D256 |
Total Impact Polystyrene 940E Super High Impact Polystyrene, Sheet Extrusion and Thermoforming Grade TOTAL Petrochemicals 940E is a super high impact polystyrene designed for high gloss sheet extrusion and thermoforming applications that require additional toughness.Applications: The combination o.. |