Polymer Property : Impact Test = 24.9 J
Polymer Property :
Impact Test =
24.9 J
Product List
Mechanical Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties
Metric
English
Comments
Impact Test
24.9
J
18.3
ft-lb
ID Impact @ 5mph, Peak Energy; ASTM D3763-86
Dow TF0807 TPO
Dow Fascia TPO for Painted ApplicationsInformation provided by Dow