Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Impact Test | 4.76 J | 3.51 ft-lb | Multi-Axial Instrumented Impact Energy; ISO 6603-2 |
LNP Lubricomp® QFL-4017 ER HS Polyamide 6/10 Copolymer, Glass Fiber Reinforcement, PTFE Lubricant
(discontinu Features: Heat Stabilized, Good Mold Release, LubricatedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; .. |