Polymer Property : Impact Test = 31.2 J Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Impact Test 31.2 J

@Temperature -40.0 °C
23.0 ft-lb

@Temperature -40.0 °F
Instrumented Impact, Total Energy; ASTM D3763
ExxonMobil LD 051.LJ Molding, Extrusion and Compounding Resin  (discontinued **)
LD 051.LJ resin is used in Blow molded, squeeze bottles, Pail lids, Closures, and Extruded profiles.Information provided by ExxonMobil Chemical
Impact Test 31.2 J

@Temperature -20.0 °C
23.0 ft-lb

@Temperature -4.00 °F
Cold Temperature Impact Energy; ASTM D3763
Total Lumicene® mPE BM359 SG Metallocene Medium Density High Gloss Blow Molding Resin
Metallocene Medium Density High Gloss Blow Molding ResinCharacteristics:Outstanding glossGood flexibilityExcellent impact strengthGood ESCRUSP Class VI compliantFDA CompliantApplications:Coextruded ..