Impact Test 44.7 J

@Temperature 22.8 °C
33.0 ft-lb

@Temperature 73.0 °F
Dynatup Instrumented Impact; ASTM D3763
Spartech Royalite DKE 400 PVC/Acrylic Fire Rated Sheet
Description: Fire Rated SheetInformation provided by Spartech.
Impact Test 44.7 J

@Temperature 22.8 °C
33.0 ft-lb

@Temperature 73.0 °F
Dynatup Instrumented Impact; ASTM D3763
Spartech Royalite R52 PVC/Acrylic Fire Rated Sheet
Description: Fire Rated SheetInformation provided by Spartech.