Mechanical Properties Metric English Comments
Impact Test 45.0 J

@Temperature 23.0 °C
33.2 ft-lb

@Temperature 73.4 °F
Instrumented Impact Total Energy; ASTM D 3763
SABIC Innovative Plastics Cycoloy® CM6210 PC+ABS (Europe-Africa-Middle East)
Cycoloy* resin CM6210 is a high-modulus flame retardant PC/ABS with non-brominated and non-chlorinated FR system. It can be used for extrusion & thermoforming applications and also for injection mol..
Impact Test 45.0 J

@Temperature 23.0 °C
33.2 ft-lb

@Temperature 73.4 °F
Instrumented Dart Total Energy
Dow Isoplast® 2520 Polyurethane (PUR-RT), Impact Modified  (discontinued **)
ISOPLAST® 2520 resin is an impact modified amorphous polymer with the chemical resistance of crystalline resins specially designed for medical applications. Its outstanding properties include excel..
Impact Test 45.0 J
33.2 ft-lb
Multiaxial Impact; ISO 6603
SABIC Innovative Plastics LNP LUBRILOY D20001 PPO
LNP* LUBRILOY* Z20001 is a compound based on PPO resin containing Proprietary Lubricant. Added features of this material include: Wear Resistant, Flame Retardant.
Impact Test 45.0 J

@Temperature 23.0 °C
33.2 ft-lb

@Temperature 73.4 °F
Instrumented Dart Total Energy
Styron Magnumâ„¢ 2610 ABS, High Gloss
MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM ..
Impact Test 45.0 J

@Temperature 23.0 °C
33.2 ft-lb

@Temperature 73.4 °F
Instrumented Dart Total Energy
Styron Magnumâ„¢ 780HP ABS, High Heat, High Impact
MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM ..
Impact Test 45.0 J

@Temperature 23.0 °C
33.2 ft-lb

@Temperature 73.4 °F
Instrumented Dart Total Energy
Styron Magnumâ„¢ 9010 ABS, High Gloss
MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM ..
Impact Test 45.0 J

@Temperature 23.0 °C
33.2 ft-lb

@Temperature 73.4 °F
Instrumented Dart Total Energy
Styron Magnumâ„¢ 9450P ABS, High Gloss
MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM ..
Impact Test 45.0 J

@Temperature 23.0 °C
33.2 ft-lb

@Temperature 73.4 °F
Instrumented Impact Total Energy; ASTM D 3763
SABIC Innovative Plastics Noryl N1251 PPE+PS
ECO-FLO(tm). ECO conforming, non-halogen flame retardant PPE+PS. High flow. Electrical and Business Equipment applications.This data was supplied by SABIC-IP for the Americas region.
Impact Test 45.0 J

@Temperature 23.0 °C
33.2 ft-lb

@Temperature 73.4 °F
Instrumented Impact Total Energy; ASTM D 3763
SABIC Innovative Plastics Xenoy® X5630 PC+PET
Mineral filled PC/PET blend with high heat dimensional stability, low shrinkage and low CTE, especially for painted applicationsThis data was supplied by SABIC-IP for the Americas region.
Impact Test 45.0 J

@Temperature 23.0 °C
33.2 ft-lb

@Temperature 73.4 °F
Instrumented Dart Total Energy
Styron Magnumâ„¢ 344HP ABS
MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM ..
Impact Test 45.0 J

@Thickness 3.20 mm
33.2 ft-lb

@Thickness 0.126 in
Instrumented Total Impact; 3.2 mm thick, 12.5 mm dart, 75 mm clamp, 6.7 m/s; ASTM D3763
Covestro Bayblend® T 85 Polycarbonate/ABS Blend
High impact and notched impact strength, little risk of brittle fracture, high dimensional accuracy.Applications: Automotive components, electrical engineering.Information provided by Bayer.As of 1 ..
Impact Test 45.0 J

@Thickness 3.20 mm
33.2 ft-lb

@Thickness 0.126 in
Instrumented Total Impact; 12.5 mm dart, 75 mm clamp, 6.7 m/s; ASTM D3763
Covestro Bayblend® T 88-2N Polycarbonate/ABS Blend, 10% Glass Fiber
Contains 10% glass fiber reinforcement, high stiffness.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – ..
Impact Test 45.0 J

@Thickness 3.20 mm
33.2 ft-lb

@Thickness 0.126 in
Instrumented Impact, Total Energy; 3.2 mm thick, 7.6 mph, 1.5 in. clamp, 0.5 in. dart; ASTM D3763
Covestro Bayblend® 2253 Polycarbonate + ABS Blend, Extrusion  (discontinued **)
Properties tested in transverse direction (worst case) on 125-mil (3.2 mm) extruded sheets specimens with
Impact Test 45.0 J

@Temperature 23.0 °C
33.2 ft-lb

@Temperature 73.4 °F
Instrumented Dart Total Energy
Styron Magnum™ 3490 ABS, High Gloss
MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM AB..
Impact Test 45.0 J
33.2 ft-lb
Multiaxial Impact; ISO 6603
SABIC Innovative Plastics LNP LUBRILOY Z20001 PPO
LNP* Lubriloy* Z20001 is a compound based on PPE+PS Blend resin containing Proprietary Lubricant. Added features of this material include: Wear Resistant, Flame Retardant.