Impact Test 48.8 J

@Temperature 22.8 °C
36.0 ft-lb

@Temperature 73.0 °F
Dynatup Instrumented Impact; ASTM D3763
Spartech Royalite R60 PVC/Acrylic Aircraft Grade Sheet
Description: Aircraft Grade SheetInformation provided by Spartech.
Impact Test 48.8 J

@Temperature -29.0 °C
36.0 ft-lb

@Temperature -20.2 °F
ASTM D3763
Braskem TI4003F Impact Copolymer Polypropylene
Description: Extra High Izod Impact, Very High Flexural Modulus, Good Low Temperature Drop ImpactApplications: Suggested Uses Include Blow Molding, Extrusion, Profiles, PipeThis resin meets the requ..
Impact Test 48.8 J

@Temperature -29.0 °C
36.0 ft-lb

@Temperature -20.2 °F
ASTM D3763
Braskem TI4005F Impact copolymer Polypropylene
Description: Extra high izod impact, very high flexural modulus, good low temperature drop impact.Applications: Suggested uses include compounding and thermoforming.Process: Thermoforming.This resin..
Impact Test 48.8 J
36.0 ft-lb
ASTM D3763
Braskem TI4130G Impact Copolymer Polypropylene
Description: Medium izod impact, good blush resistance, good low temperature drop impact.Applications: Suggested uses include furniture, housewares, automotive interior trim. UL temperature index of..
Impact Test 48.8 J

@Temperature -29.0 °C
36.0 ft-lb

@Temperature -20.2 °F
ASTM D3763
Braskem TI6500WV High Impact Copolymer Polypropylene
Description: High melt flow, superior low temperature impact, nucleated, good mold release, antistatic.Applications: Suggested uses include compounding, furniture, toys, packaging, large part inject..