Impact Test 42.0 J

@Thickness 2.50 mm
31.0 ft-lb

@Thickness 0.0984 in
Instrumented Total Impact; 2.5 mm thick, 12.5 mm dart, 40 mm clamp, 3.3 m/s; ASTM D3763
Ineos ABS TRIAX® 1120 ABS/Nylon Blend, Injection Grade, As Conditioned
Injection molding grade with good flow and stress corrosion cracking resistance, good chemical resistance (fuel, cleaning agents), high impact and notched impact strength, good acoustical damping be..
Impact Test 42.0 J
31.0 ft-lb
Multiaxial Impact; ISO 6603
SABIC Innovative Plastics LNP LUBRILOY D2000 PC
LNP LUBRILOY* D2000 is a compound based on Polycarbonate resin containing Proprietary Lubricant. Added feature of this material is: Wear Resistant.
Impact Test 42.0 J

@Temperature 22.8 °C
31.0 ft-lb

@Temperature 73.0 °F
Dynatup Instrumented Impact; ASTM D3763
Spartech Royalite R910 PC/ABS General Purpose Sheet
Description: General Purpose SheetInformation provided by Spartech.
Impact Test 42.0 J

@Temperature 23.0 °C
31.0 ft-lb

@Temperature 73.4 °F
Instrumented Dart Total Energy
Styron Magnumâ„¢ 758HP ABS, High Heat, High Impact
MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM ..
Impact Test 42.0 J

@Temperature 23.0 °C
31.0 ft-lb

@Temperature 73.4 °F
Instrumented Impact Total Energy; ASTM D 3763
SABIC Innovative Plastics Noryl FXN119LG PPE+HIPS
Noryl FXN119LG is a low gloss PPE/HIPS grade. It provides a balance of mechanical properties and heat performance with intrinsic low gloss appreance. FXN119LG is available in mutliple colors.This da..
Impact Test 42.0 J

@Temperature 23.0 °C
31.0 ft-lb

@Temperature 73.4 °F
Instrumented Impact Total Energy; ASTM D 3763
SABIC Innovative Plastics Noryl FXN119LG PPE+HIPS (Asia Pacific)
Noryl FXN119LG is a low gloss PPE/HIPS grade. It provides a balance of mechanical properties and heat performance with intrinsic low gloss appreance. FXN119LG is available in mutliple colors.This da..
Impact Test 42.0 J

@Temperature 23.0 °C
31.0 ft-lb

@Temperature 73.4 °F
Instrumented Impact Total Energy; ASTM D 3763
SABIC Innovative Plastics Noryl FXN119LG PPE+HIPS (Europe-Africa-Middle East)
Noryl FXN119LG is a low gloss PPE/HIPS grade. It provides a balance of mechanical properties and heat performance with intrinsic low gloss appreance. FXN119LG is available in mutliple colors.This da..