Mechanical Properties Metric English Comments
Impact Test 46.1 J

@Temperature 4.00 °C
34.0 ft-lb

@Temperature 39.2 °F
ASTM D3763
Braskem TI4040WT Impact Copolymer Polypropylene
Description: Superior drop impact at refrigeration temperature, very high flexural modulus, nucleated, good mold release.Applications: Suggested uses include thermoforming, food packaging, dairy con..