Mechanical Properties Metric English Comments
Impact Test 65.1 J

@Thickness 3.17 mm,
Temperature -40.0 °C
48.0 ft-lb

@Thickness 0.125 in,
Temperature -40.0 °F
ARM impact
A. Schulman POLYAXIS® CP812 Stabilized Compounded Rotational Molding Resin
DescriptionPolyaxis CP 812 is a stabilized compounded rotational molding resin with a combination of good flow and stiffness. NOTE: Physical properties are based on rotationally molded samples from ..
Impact Test 65.1 J

@Thickness 3.17 mm,
Temperature -40.0 °C
48.0 ft-lb

@Thickness 0.125 in,
Temperature -40.0 °F
ARM impact
A. Schulman POLYAXIS® CP812 Stabilized Compounded Rotational Molding Resin
DescriptionPolyaxis CP 812 is a stabilized compounded rotational molding resin with a combination of good flow and stiffness. NOTE: Physical properties are based on rotationally molded samples from ..
Impact Test 65.1 J

@Thickness 3.17 mm,
Temperature -40.0 °C
48.0 ft-lb

@Thickness 0.125 in,
Temperature -40.0 °F
ARM impact
A. Schulman POLYAXIS® CP812 Stabilized Compounded Rotational Molding Resin
DescriptionPolyaxis CP 812 is a stabilized compounded rotational molding resin with a combination of good flow and stiffness. NOTE: Physical properties are based on rotationally molded samples from ..
Impact Test 65.1 J

@Thickness 3.17 mm,
Temperature -40.0 °C
48.0 ft-lb

@Thickness 0.125 in,
Temperature -40.0 °F
ARM impact
A. Schulman POLYAXIS® CP812 Stabilized Compounded Rotational Molding Resin
DescriptionPolyaxis CP 812 is a stabilized compounded rotational molding resin with a combination of good flow and stiffness. NOTE: Physical properties are based on rotationally molded samples from ..
Impact Test 65.1 J

@Thickness 3.17 mm,
Temperature -40.0 °C
48.0 ft-lb

@Thickness 0.125 in,
Temperature -40.0 °F
ARM impact
A. Schulman POLYAXIS® CP812 Stabilized Compounded Rotational Molding Resin
DescriptionPolyaxis CP 812 is a stabilized compounded rotational molding resin with a combination of good flow and stiffness. NOTE: Physical properties are based on rotationally molded samples from ..
Impact Test 65.1 J

@Thickness 3.17 mm,
Temperature -40.0 °C
48.0 ft-lb

@Thickness 0.125 in,
Temperature -40.0 °F
ARM impact
A. Schulman POLYAXIS® CP812 Stabilized Compounded Rotational Molding Resin
DescriptionPolyaxis CP 812 is a stabilized compounded rotational molding resin with a combination of good flow and stiffness. NOTE: Physical properties are based on rotationally molded samples from ..
Copyright © lookpolymers.com All Rights Reserved