Polymer Property : Impact Test = 5.34 ft-lb Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Impact Test 7.24 J
5.34 ft-lb
Max. Energy; Dynatup
KYDEX® 6503 Integral Pearlescent Low Heat Release Aviation Thermoforming Sheet
Features:Thicknesses from 0.71 mm to 3.18 mmChemical resistant - easy to clean with aggressive cleanersForms deep draws with low forces when heated to the upper end of forming temperature rangeCrisp..
Impact Test 7.24 J
5.34 ft-lb
Dynatup Max Energy
KYDEX® 6565 Acrylic/PVC Thermoplastic Sheet
Low heat release aviation gradeApplications: Airducts, seat parts, bulkhead laminates, escape slide packboards, gallery parts, instrument panels, laboratory floorplans, sidewall panels, life vest sh..