Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Impact Test | 7.91 J | 5.83 ft-lb | Reverse; ASTM D2794 |
Chesterton ARC MX2 High Wear Fine Particle Wear Compound Description: An advanced ceramic composite for the repair and protection of all metal surfaces subjected to severe erosion, corrosion and chemical attack. It is applied at a thickness of 3 mm (1/8”.. |