Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Impact Test | 75.0 J @Temperature 23.0 °C |
55.3 ft-lb @Temperature 73.4 °F |
Instrumented Impact Total Energy; ASTM D 3763 |
SABIC Innovative Plastics Lexan® EXL1484T PC Copolymer Lexan* EXL1484T polycarbonate (PC) siloxane copolymer resin is a UV stabilized, enhanced release transparent injection molding grade. This resin offers extreme low temperature (-40 C) ductility in c.. |
|||
Impact Test | 75.0 J @Temperature 23.0 °C |
55.3 ft-lb @Temperature 73.4 °F |
Instrumented Impact Total Energy; ASTM D 3763 |
SABIC Innovative Plastics Lexan® FXE1414T PC Copolymer (Europe-Africa-Middle East) Clear PC-siloxane copolymer with excellent processability, for Visual fX capability in "Energy" colors. Medium flow. Improved toughness compared to medium flow standard PC in same color. Color packa.. |
|||
Impact Test | 75.0 J @Temperature 23.0 °C |
55.3 ft-lb @Temperature 73.4 °F |
Instrumented Impact Total Energy; ASTM D 3763 |
SABIC Innovative Plastics Lexan® EXL1033C PC Copolymer Lexan*EXL1033C polycarbonate (PC) siloxane copolymer resin is a low flow, UV stabilized grade designed for (co)-extrusion. This resin offers low temperature (-30C) ductility and excellent extrusion .. |
|||
Impact Test | 75.0 J @Temperature 23.0 °C |
55.3 ft-lb @Temperature 73.4 °F |
Instrumented Impact Total Energy; ASTM D 3763 |
SABIC Innovative Plastics Lexan® FXE1434T PC Copolymer (Europe-Africa-Middle East) Lexan* EXL1434T polycarbonate (PC) siloxane copolymer resin is a UV stabilized transparent injection molding grade. This resin offers extreme low temperature (-40 C) ductility in combination with me.. |