Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Impact Test 90.4 J

@Temperature 23.0 °C
66.7 ft-lb

@Temperature 73.4 °F
Instrumented Dart Total Energy
Styron CALIBREâ„¢ 200 6 Polycarbonate, General Purpose
CALIBRE® 200 series are general purpose, UL listed Polycarbonate resins formulated to comply with the applicable FDA and European regulations governing food contact(1). CALIBRE 200 series resins ..
Impact Test 90.4 J

@Temperature 23.0 °C
66.7 ft-lb

@Temperature 73.4 °F
Instrumented Dart Total Energy
Styron CALIBREâ„¢ 300 6 Polycarbonate, General Purpose
CALIBRE® 300 series are general purpose, UL listed polycarbonate resins. CALIBRE 300 series resins exhibit an excellent physical property balance of heat resistance, transparency and impact stren..