Polymer Property : Impact Test = 70.0 J Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Impact Test 70.0 J
51.6 ft-lb
Multiaxial Impact; ISO 6603
SABIC Innovative Plastics Cycoloy® CX1440 PC+ABS
CYCOLOY CX1440 is a general purpose PC+ABS blend specially developped for thin wall applications requiring weld line strength and high flow with a good balance of properties
Impact Test 70.0 J
51.6 ft-lb
Multiaxial Impact; ISO 6603
SABIC Innovative Plastics Cycoloy® CX1440 PC+ABS (Europe-Africa-Middle East)
CYCOLOY CX1440 is a general purpose PC+ABS blend specially developped for thin wall applications requiring weld line strength and high flow with a good balance of propertiesThis data was supplied by..
Impact Test 70.0 J

@Temperature 23.0 °C
51.6 ft-lb

@Temperature 73.4 °F
Instrumented Impact Total Energy; ASTM D 3763
SABIC Innovative Plastics Lexan® EXL1192C PC Copolymer
High flow, polycarbonate siloxane copolymer resin. Notched izod ductile to -20C ductility. Enhanced processability compared to standard PC resins. Available in a range of transparent colors. US ..
Impact Test 70.0 J

@Temperature 23.0 °C
51.6 ft-lb

@Temperature 73.4 °F
Instrumented Impact Total Energy; ASTM D 3763
SABIC Innovative Plastics Lexan® EXL1444 PC Copolymer (Europe-Africa-Middle East)
Lexan* EXL1444 polycarbonate (PC) siloxane copolymer resin is a medium flow opaque injection molding (IM) grade suitable for FDA compliant applications. This resin offers extreme low temperature (-..
Impact Test 70.0 J

@Temperature 23.0 °C
51.6 ft-lb

@Temperature 73.4 °F
Instrumented Impact Total Energy; ASTM D 3763
SABIC Innovative Plastics Lexan® FXD171R PC
Transparent/transluscent PC for light diffusion special effects. MFR of 25.0.This data was supplied by SABIC-IP for the Americas region.
Impact Test 70.0 J

@Temperature 23.0 °C
51.6 ft-lb

@Temperature 73.4 °F
Instrumented Impact Total Energy; ASTM D 3763
SABIC Innovative Plastics Lexan® ML6018R PC (Asia Pacific)
ML6018R is a low viscosity grade exhibiting a high impact performance over standard PC. It contains an enhanced release-agent. Opaque colours only.This data was supplied by SABIC-IP for the Asia Pac..
Impact Test 70.0 J

@Temperature 23.0 °C
51.6 ft-lb

@Temperature 73.4 °F
Instrumented Impact Total Energy; ASTM D 3763
SABIC Innovative Plastics Xenoy® X4810 PBT+PC
Xenoy X4810 is a hydrostable, High Modulus Ductile PC/PBT blend. This resin provides low temperature (below 0C) ductile impact behaviour, high chemical resistance, very low creep, low CTE, excellent..
Impact Test 70.0 J

@Temperature -20.0 °C
51.6 ft-lb

@Temperature -4.00 °F
Instrumented Impact Total Energy; ASTM D 3763
SABIC Innovative Plastics Xenoy® X4810 PBT+PC
Xenoy X4810 is a hydrostable, High Modulus Ductile PC/PBT blend. This resin provides low temperature (below 0C) ductile impact behaviour, high chemical resistance, very low creep, low CTE, excellent..
Impact Test 70.0 J
51.6 ft-lb
Multiaxial Impact; ISO 6603
SABIC Innovative Plastics Noryl GTX LMX171 PPO/PBT (Europe-Africa-Middle East)
Noryl LMX171 is a PPO/PBT blend including conductive agent with a balanced heat/impact property profile. Noryl LMX differentiate from Noryl GTX by a lower moisture uptake (0.15%).This data was suppl..
Impact Test 70.0 J
51.6 ft-lb
Multiaxial Impact; ISO 6603
SABIC Innovative Plastics LNP Stat-kon FX97333 PE
LNP* Stat-kon* FX97333 is a compound based on Polyethylene resin containing Carbon Powder. Added features of this material include: Electrically Conductive.This data was supplied by SABIC-IP for th..
Impact Test 70.0 J
51.6 ft-lb
Multiaxial Impact; ISO 6603
SABIC Innovative Plastics LNP Stat-kon FX97333 PE (Asia Pacific)
LNP* Stat-kon* FX97333 is a compound based on Polyethylene resin containing Carbon Powder. Added features of this material include: Electrically Conductive.This data was supplied by SABIC-IP for th..
Impact Test 70.0 J

@Temperature 23.0 °C
51.6 ft-lb

@Temperature 73.4 °F
Instrumented Impact Total Energy; ASTM D 3763
SABIC Innovative Plastics Xylex X7529 PC+POLYESTER (Asia Pacific)
PC+ POLYESTER unreinforced alloy developed for optical or lense market. Good flow with good impact and excellent optical quality. UV 400nm block.This data was supplied by SABIC-IP for the Asia Pacif..
Impact Test 70.0 J

@Temperature 23.0 °C
51.6 ft-lb

@Temperature 73.4 °F
Instrumented Impact Total Energy; ASTM D 3763
SABIC Innovative Plastics Xylex X7529 PC+POLYESTER (Europe-Africa-Middle East)
PC+ POLYESTER unreinforced alloy developed for optical or lense market. Good flow with good impact and excellent optical quality. UV 400nm block.This data was supplied by SABIC-IP for the Europe-Afr..
Impact Test 70.0 J

@Temperature 23.0 °C
51.6 ft-lb

@Temperature 73.4 °F
Instrumented Impact Total Energy; ASTM D 3763
SABIC Innovative Plastics Xylex X7529OQ PC+POLYESTER (Europe-Africa-Middle East)
PC+ POLYESTER unreinforced alloy developed for optical or lense market. Good flow with good impact and excellent optical qualityThis data was supplied by SABIC-IP for the Europe-Africa-Middle East r..
Impact Test 70.0 J
51.6 ft-lb
Multiaxial Impact; ISO 6603
SABIC Innovative Plastics Cycoloy® CX1440 PC+ABS (Asia Pacific)
CYCOLOY CX1440 is a general purpose PC+ABS blend specially developped for thin wall applications requiring weld line strength and high flow with a good balance of properties
Impact Test 70.0 J

@Temperature 23.0 °C
51.6 ft-lb

@Temperature 73.4 °F
Instrumented Impact Total Energy; ASTM D 3763
SABIC Innovative Plastics Xylex X7529OQ PC+POLYESTER (Asia Pacific)
PC+ POLYESTER unreinforced alloy developed for optical or lense market. Good flow with good impact and excellent optical qualityThis data was supplied by SABIC-IP for the Asia Pacific region.