Polymer Property : Impact Test = 80.0 ft-lb Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Impact Test 108 J

@Thickness 3.17 mm,
Temperature -40.0 °C
80.0 ft-lb

@Thickness 0.125 in,
Temperature -40.0 °F
ARM
ExxonMobil HDPE HD 8660.29 High Density Polyethylene Resin
Product Description: HD 8660 series are high density hexane copolymers designed to offer superior toughness and stiffness. They are ideally suited for applications that require the optimum balance o..
Impact Test 108 J

@Thickness 3.17 mm,
Temperature -40.0 °C
80.0 ft-lb

@Thickness 0.125 in,
Temperature -40.0 °F
ARM
ExxonMobil HDPE HD P8660.29 High Density Polyethylene Resin
Product Description: HD 8660 series are high density hexane copolymers designed to offer superior toughness and stiffness. They are ideally suited for applications that require the optimum balance o..