Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Impact Test | 81.3 J | 60.0 ft-lb | Torque Strength; curing at 1000°F |
Aremco Ceramabond™ 670 High Temperature Ceramic Adhesive/Paste, Alumina Filled Aremco's ceramic adhesives are easy to use, one- and two-component systems which air dry in 1-2 hrs and are ready for use following a 200 to 700 °F cure. These materials are mostly water-based and.. |
|||
Impact Test | 81.3 J | 60.0 ft-lb | Torque Strength; curing at 1000°F |
Aremco Ceramabond™ 503 High Temperature Ceramic Adhesive/Paste, Alumina Filled Aremco's ceramic adhesives are easy to use, one- and two-component systems which air dry in 1-2 hrs and are ready for use following a 200 to 700 °F cure. These materials are mostly water-based and.. |
|||
Impact Test | 81.3 J @Thickness 3.17 mm, Temperature -40.0 °C |
60.0 ft-lb @Thickness 0.125 in, Temperature -40.0 °F |
Low Temperature; ARM |
Formosa Plastics Formolene® L64220U Rotational Molding LLDPE
(discontinued **) Linear Low Density Polyethylene Hexene Copolymer for Rotational Molding Formolene® L64220U is a general-purpose rotational molding linear low density resin made using the BP Gas Phase ProcessTM. Th.. |