Impact Test 130.65 J
96.362 ft-lb
Cum. Energy; Dynatup
KYDEX® 6503 Integral Pearlescent Low Heat Release Aviation Thermoforming Sheet
Features:Thicknesses from 0.71 mm to 3.18 mmChemical resistant - easy to clean with aggressive cleanersForms deep draws with low forces when heated to the upper end of forming temperature rangeCrisp..