Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Hot Tack Strength | 1250 g/25 mm | 1250 g/in | seal bar 110°C; Packforsk method. |
DuPont Nucrel® 30707HS Ethylene-Acrylic Acid Copolymer Resin for Film and Extrusion Coating
(discontinued **) 7 wt% Acrylic Acid.Nucrel® 30707HS is an ethylene-acrylic acid copolymer resin available for use in blown/cast film and extrusion coating operations. It can be used in both extrusion and coextrusio.. |