Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Hot Tack Strength | <= 2200 g/25 mm | <= 2200 g/in | Varies with seal bar temp.; Packforsk Method |
DuPont™ Surlyn® 1705-1 Zinc Ionomer Resin for Blown and Cast Film Surlyn® 1705-1 is an ionomer resin available for use in conventional blown and cast film extrusion and coextrusion equipment designed to process polyethylene resins. Applications: Meat, poultry, s.. |