Polymer Property : Hot Tack Strength = 2400 g/25 mm Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Hot Tack Strength 2400 g/25 mm
2400 g/in
Seal Bar Temp approx. 115-135°C; Packforsk Method
DuPont™ Surlyn® 1650 Zinc Ionomer Resin for Blown and Cast Film
Surlyn® 1650 is an ionomer resin available for use in conventional blown and cast film extrusion and coextrusion equipment designed to process polyethylene resins. Applications: Meat, poultry, sea..