Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.170 J/cm @Temperature -30.0 °C |
0.318 ft-lb/in @Temperature -22.0 °F |
ASTM D 256 |
SABIC Innovative Plastics Noryl PX0346 PPE+PS This data was supplied by SABIC-IP for the Americas region. |