Polymer Property : Izod Impact, Notched = 0.420 J/cm Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 0.420 J/cm

@Thickness 4.00 mm,
Temperature -20.0 °C
0.787 ft-lb/in

@Thickness 0.157 in,
Temperature -4.00 °F
ISO 180
Premix Thermoplastics PRE-ELEC® PS 1326
PRE-ELEC PS 1326 is a conductive thermoplastic compound based on polystyrene. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELEC ..
Izod Impact, Notched 0.420 J/cm

@Temperature -30.0 °C
0.787 ft-lb/in

@Temperature -22.0 °F
ASTM D 256
SABIC Innovative Plastics Geloy XTWE280 ASA
Weatherble ASA profile extrusion gradeThis data was supplied by SABIC-IP for the Americas region.
Izod Impact, Notched 0.420 J/cm

@Temperature -30.0 °C
0.787 ft-lb/in

@Temperature -22.0 °F
ASTM D 256
SABIC Innovative Plastics Geloy XTWE280 ASA (Europe-Africa-Middle East)
Weatherble ASA profile extrusion gradeThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Izod Impact, Notched 0.420 J/cm

@Temperature 23.0 °C
0.787 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
SABIC Innovative Plastics Lexan® DMX9254 PC
Lexan* DMX9254 resin is an injection moldable PC copolymer/ABS blend. This resin combines excellent scratch resistance with high flow and ductility. It contains non-brominated and non-chlorinated fl..
Izod Impact, Notched 0.420 J/cm

@Temperature 23.0 °C
0.787 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
SABIC Innovative Plastics Lexan® DMX9254 PC (Asia Pacific)
Lexan* DMX9254 resin is an injection moldable PC copolymer/ABS blend. This resin combines excellent scratch resistance with high flow and ductility. It contains non-brominated and non-chlorinated fl..
Izod Impact, Notched 0.420 J/cm

@Temperature 23.0 °C
0.787 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
SABIC Innovative Plastics Lexan® DMX9254 PC (Europe-Africa-Middle East)
Lexan* DMX9254 resin is an injection moldable PC copolymer/ABS blend. This resin combines excellent scratch resistance with high flow and ductility. It contains non-brominated and non-chlorinated fl..
Izod Impact, Notched 0.420 J/cm

@Temperature -30.0 °C
0.787 ft-lb/in

@Temperature -22.0 °F
ASTM D 256
SABIC Innovative Plastics Geloy XTWE280 ASA (Asia Pacific)
Weatherble ASA profile extrusion gradeThis data was supplied by SABIC-IP for the Asia Pacific region.