Mechanical Properties Metric English Comments
Izod Impact, Notched 0.44145 J/cm

@Temperature -20.0 °C
0.82702 ft-lb/in

@Temperature -4.00 °F
JIS-K-6740
Denka VINYKON R2001 PVC, R grade for hard extrusion
A PVC resin compound offering excellent physical properties and workability. A broad product lineup is available, including hard and soft grades, as well as those for extrusion and injection molding..
Izod Impact, Notched 0.44145 J/cm

@Temperature -20.0 °C
0.82702 ft-lb/in

@Temperature -4.00 °F
JIS-K-6740
Denka VINYKON R3105 PVC, R grade for hard extrusion
A PVC resin compound offering excellent physical properties and workability. A broad product lineup is available, including hard and soft grades, as well as those for extrusion and injection molding..
Izod Impact, Notched 0.44145 J/cm

@Temperature -20.0 °C
0.82702 ft-lb/in

@Temperature -4.00 °F
JIS-K-6740
Denka VINYKON R3102 PVC, R grade for hard extrusion
A PVC resin compound offering excellent physical properties and workability. A broad product lineup is available, including hard and soft grades, as well as those for extrusion and injection molding..