Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Izod Impact, Notched = 0.510 J/cm Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 0.510 J/cm

@Temperature 23.0 °C
0.955 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Eastman 7352 PET  (discontinued **)
VORIDIAN PET thermoplastic polyesters are condensation polymers produced by a continuous melt-phase polymerization process followed by a solid-state polymerization process. VORIDIAN PET polyester 73..
Izod Impact, Notched 0.510 J/cm

@Thickness 3.17 mm
0.955 ft-lb/in

@Thickness 0.125 in
ASTM D256
Samsung Cheil Industries Starex® GR-5020T SAN, 20% Glass Filled
Information provided by Samsung Cheil Industries.
Izod Impact, Notched 0.510 J/cm

@Thickness 3.17 mm
0.955 ft-lb/in

@Thickness 0.125 in
ASTM D256
Samsung Cheil Industries Starex® GR-5020T SAN, 20% Glass Filled
Information provided by Samsung Cheil Industries.
Izod Impact, Notched 0.510 J/cm

@Temperature 23.0 °C
0.955 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Eastman Eastar EN052 Polyester
Eastar Polyester EN052 is a thermoplastic condensation homopolymer produced by a continuous melt-phase polymerization process followed by a solid-state polymerization process. It has been crystalliz..
Izod Impact, Notched 0.510 J/cm

@Temperature 23.0 °C
0.955 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Eastman Eastar MN052 Polyester, Natural
Eastar polyester MN052 is a thermoplastic condensation homopolymer produced by a continuous melt-phase polymerization process followed by a solid-state polymerization process. It has been crystalliz..
Copyright © lookpolymers.com All Rights Reserved