Polymer Property : Izod Impact, Notched = 0.579 J/cm Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 0.579 J/cm

@Thickness 6.35 mm
1.08 ft-lb/in

@Thickness 0.250 in
ASTM D256
Samsung Cheil Industries Infino® VB-5300GS PBT, Glass Filled FR
Information provided by Samsung Cheil Industries.
Izod Impact, Notched 0.579 J/cm

@Thickness 6.35 mm
1.08 ft-lb/in

@Thickness 0.250 in
ASTM D256
Samsung Cheil Industries Infino® VB-5300GS PBT, Glass Filled FR
Information provided by Samsung Cheil Industries.