Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.320 J/cm @Temperature -30.0 °C |
0.600 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
Formosa Plastics Formolene® 6335N Impact Copolymer Polypropylene Impact Copolymer - Designed to Meet the Physical Requirements of Automotive Interior Trim Formolene® 6335N is an engineered, medium impact copolymer polypropylene. It was specifically developed to.. |
|||
Izod Impact, Notched | 0.320 J/cm @Thickness 3.17 mm, Temperature -20.0 °C |
0.600 ft-lb/in @Thickness 0.125 in, Temperature -4.00 °F |
ASTM D-256 |
Axiall LR-5009 Rigid PVC, Molding, All Colors Georgia Gulf LR-5009 is an economical high flow rigid PVC fittings compound designed for multi-cavity molds and large diameter fittings. This compound is characterized by excellent process ability,.. |
|||
Izod Impact, Notched | 0.320 J/cm @Thickness 6.35 mm, Temperature -20.0 °C |
0.600 ft-lb/in @Thickness 0.250 in, Temperature -4.00 °F |
ASTM D-256 |
Axiall 5009 Rigid PVC, Molding Georgia Gulf 5009 is a type I, Grade I rigid vinyl injection molding compound designed for fittings and parts of similar confiation where maximum tensile strength and/or chemical resistance is requi.. |